Creepage Distance from 10.4 mm to 3.5 mm: How JA's DeepBlue 5.0 Builds a New IEC 61730 Clause into the Frame

At TaiyangNews' Reliable PV Module Design conference, JA presented DeepBlue 5.0: butyl sealant in the frame slots forms a cemented joint that cuts the minimum creepage distance from about 10.4 mm to 3.5 mm, with the module reportedly certified to IEC 61730-1:2023. Other features include triple-cut G12R cells with gapless interconnection, a ribbon section moved to the rear (saving ~25 mm), a triangular rear-glass hole layout, and a TÜV Rheinland Class A+ partial shading rating. We summarize the key points and the reliability questions behind the numbers.
On November 9, TaiyangNews published a write-up of a talk by JA Product Manager Djamel Eddine Mansour at its Reliable PV Module Design online conference. What caught our attention most: JA applies butyl sealant in the frame slots to form what the standard calls a cemented joint, cutting the minimum creepage distance from the cell to the module edge from the usual ~10.4 mm to 3.5 mm. In this news brief, we walk through the key points and share our view.
01 What was announced, at a glance
Below are the key facts from the report. Note that all of these come from the conference write-up; we have not seen the certificates themselves.
| Item | As reported |
|---|---|
| Product | DeepBlue 5.0 TOPCon module, in mass production since Q2 2026 |
| Cell | G12R TOPCon "Bycium+ 5.0", cut into three equal slices along the length |
| Format | 2,382 × 1,134 mm |
| Interconnection | Gapless overlap of cut edges, with buffer film between strips |
| Ribbon section | Moved to the rear side, saving ~25 mm of module length |
| Edge insulation | Butyl sealant in frame slots forms a cemented joint; min. creepage 3.5 mm (vs ~10.4 mm) |
| Standard | Reportedly tested and certified to IEC 61730-1:2023 |
| Rear glass | Triangular hole layout; up to 14% less stress at holes under extreme load |
| Partial shading | Five TÜV Rheinland shading scenarios, Class A+ |
02 What creepage distance is, and why it can shrink
Creepage distance is the shortest path between two conductive parts measured along the surface of insulation. In a module, it is the distance from live cells/ribbons to accessible parts such as the frame, creeping along the encapsulation interfaces. Moisture and contamination at an interface can create a leakage path, so the standard sets minimum values based on system voltage, pollution degree and material group. Much of the ~10 mm margin at a conventional module edge exists for this reason.
The 2016 edition of IEC 61730-1 adopted the insulation coordination framework of IEC 60664, including the concept of a cemented joint: if insulating layers are reliably bonded and the interface is verified not to crack or delaminate, it is no longer treated as an ordinary surface creepage path but evaluated as distance through a cemented joint, with much lower requirements. The 2023 edition (Ed. 3) continues and refines this framework. JA's approach is to seal the glass edge with butyl in the frame slot so that this edge interface is certified as a cemented joint.

Fig. 1 Minimum creepage distance: conventional vs cemented-joint design

Fig. 2 Module edge cross-section (schematic): conventional margin vs butyl cemented joint
03 Why butyl
The report gives several reasons for choosing butyl. We explain each:
- Insulation: Butyl rubber is an insulating copolymer with stable volume resistivity, helping wet leakage current and insulation resistance.
- Compatibility: It is chemically compatible with conventional encapsulants, with little risk of interfacial reaction or exudation.
- Barrier: Its non-polar structure gives a better barrier to moisture and other gases than EVA or POE, i.e. a lower water vapor transmission rate (WVTR), blocking moisture ingress from the edges.
- Area: A narrower edge margin allows larger cells in the same format; the report cites an active-area gain of about 1%.
Butyl edge sealing is nothing new in glass-glass and thin-film modules. What is notable here is that it is not just an extra moisture barrier: it is certified as part of the safety insulation, which directly translates into a geometric gain.
Takeaway: The value of a cemented joint is not only better moisture resistance: it turns the edge margin from a safety constraint into a design parameter.
04 Other structural features
Beyond edge insulation, the report mentions several supporting designs, all pointing the same way: give more area to power generation without changing the module's outer dimensions.
- Triple-cut cells + gapless interconnection: G12R cells are cut into three slices along the length and overlapped at the cut edges, eliminating visible gaps. JA says triple cutting balances power loss, edge-passivation process stability and cutting loss; buffer film between strips absorbs field mechanical stress and reduces microcrack risk.
- Ribbon section on the rear: In conventional modules the ribbon interconnection sits on the front (middle or top/bottom edge); moving it to the rear saves about 25 mm of length.
- CSE composite structure enhancement: Keeps laminate thickness uniform between the edge and the middle, avoiding stress and sealing issues from a thinner edge.
- Triangular rear-glass holes: Ribbon holes are spread in a triangle rather than grouped centrally in a butterfly layout; JA claims up to 14% less stress at the holes under extreme mechanical load, and compatibility with various mounting structures and trackers.

Fig. 3 Length/width savings from the design features (converted from reported figures)

Fig. 4 Rear-glass hole layout (schematic): central butterfly vs distributed triangle
05 Implications for practitioners
For module design: the edge margin has long been treated as a safety constant; now there is a certification path via cemented joints. A few millimeters per edge adds up to real area and power. Other manufacturers will likely evaluate similar solutions.
For the materials supply chain: edge sealant moves from an auxiliary material to a safety insulation component. Expect clearer requirements on volume resistivity, adhesion after aging, and compatibility with encapsulants and aluminum frames, along with tighter incoming inspection and batch consistency.
For reliability and certification: a cemented joint is only valid if the interface stays bonded after aging. If the butyl debonds or cracks under damp heat, thermal cycling or mechanical load, 3.5 mm leaves no safety margin. We suggest focusing on wet leakage current and insulation resistance after aging, process control of butyl thickness and continuity during framing, and in-line detection of sealant defects in mass production.
Bottom line: 3.5 mm is the certified minimum; the real safety margin depends on whether the butyl interface stays intact for 25–30 years.
06 Our view
On value: this is a concrete case of a standard revision landing in a product. The cemented-joint provisions in IEC 61730 have existed for years, but tying them to a specific material (butyl), a specific geometry (3.5 mm) and a mass-produced module is a useful reference for the industry.
On limitations: the information so far comes only from a conference write-up. Key points remain to be verified: the IEC 61730-1:2023 certificate number and test laboratory; the specific cemented-joint test sequences and results; and the partial shading A+ certificate number, the definitions of the five shading scenarios and the rating method. The ~1% active-area gain and 14% stress reduction are also manufacturer claims without stated comparison conditions.
In the Chinese context, framing with butyl sealant differs little from existing production lines; the main barriers to adoption lie in material qualification and process control. For colleagues working on material introduction, solutions where a material doubles as a safety structure usually require the material supplier, module maker and certification body to build a solid test basis together.
07 Final thoughts
Competition on module efficiency has reached the millimeter level. JA DeepBlue 5.0's work on the edge, interconnection and rear glass follows one idea: keep the outer dimensions, and give every millimeter to power generation. And the narrower the safety margin, the more it depends on long-term material and process stability. We will follow up when certificates and more test data are published.
Calculation notes / data basis
- Creepage saving per edge: 10.4 − 3.5 = 6.9 mm (from reported figures).
- If both long edges each save 6.9 mm, the total of 13.8 mm is ~1.2% of the 1,134 mm width; if both short edges do, ~0.6% of the 2,382 mm length. These are rough geometric upper bounds; the actual active-area gain depends on the cell layout, and the report cites ~1%.
- Moving the ribbon section to the rear saves ~25 mm, about 1.0% of the 2,382 mm length (25 ÷ 2,382).
- Fig. 2 and Fig. 4 are schematics, not actual dimensions or drawings. The certificates were not available; related claims are as reported from the conference.
References
- Rajarshi Sengupta. JA: Reducing Module Creepage Distance With Cemented Joints. TaiyangNews, 2026-11-09. https://taiyangnews.info/technology/ja-topcon-creeepage-distance-cemented-joint
- IEC 61730-1:2023 Photovoltaic (PV) module safety qualification – Part 1: Requirements for construction (Ed.3, 2023-09). https://webstore.iec.ch/en/publication/25674
PV Materials Lab
https://pvmaterialslab.com
PV Materials Lab
A PV R&D and technical team with 10+ years of experience | In-depth technical knowledge sharing
Materials · Reliability · Failure Analysis · Standards & Certification · Products · Processes
Exploring AI + PV — collaboration welcome
Disclaimer:
- Original content reflects the authors' personal views only, is for reference, and does not constitute investment advice.
- Reposted and cited content is credited to its source, with respect for original work.
- Some content is AI-assisted (chart generation, data retrieval, concept explanations, etc.); the core framework and key content are written by our technical team and reviewed by humans.
- For any inaccuracy or infringement, please leave a message or contact us.