Skip to content

35.24% Perovskite/TOPCon Tandem Efficiency: Unpacking JinkoSolar’s New Record and the Four Undisclosed Metrics Engineers Must Watch ​

35.24% Perovskite/TOPCon Tandem Efficiency: Unpacking JinkoSolar’s New Record and the Four Undisclosed Metrics Engineers Must Watch

Series: Industry News & Perspectives

Key Takeaways

  • Verified Facts: On November 19, 2026, JinkoSolar announced on its official website that its N-type TOPCon-based perovskite tandem cell achieved a certified conversion efficiency of 35.24%, verified by the Shanghai Institute of Microsystem and Information Technology, Chinese Academy of Sciences (SIMIT). This marks a +0.42 percentage point (+1.21% relative) gain over its previous 34.82% record certified by the same institute five months earlier (June 16, 2026).
  • Technical Focus: The four disclosed innovations—selective passivation on textured silicon, synchronized multi-component perovskite crystallization, nanoscale interfacial passivation, and enhanced optical management—directly target the primary loss mechanisms of TOPCon-based tandems: conformal film formation on micron-scale pyramids and top/bottom subcell current matching.
  • Scope Boundaries: Key metrological parameters—active cell area, I-V scan protocol vs. steady-state MPPT output, encapsulation status, and certificate ID—were not disclosed. Until the original test certificate is publicly reviewed, this figure should not be directly benchmarked against stabilized record tables or outdoor industrial module performance.

As single-junction crystalline silicon solar cells edge closer to their ~29.4% Auger-limited theoretical ceiling, perovskite/silicon tandems have emerged as the consensus next-generation pathway. Yet for veteran PV engineers, headline lab efficiency records rarely trigger immediate celebration. Instead, they prompt three reflexive questions: What is the active area? Was it measured via fast I-V sweep or stabilized MPPT? And is the bottom cell built on an industrial textured wafer?

On November 19, 2026, JinkoSolar announced that its N-type TOPCon/perovskite tandem cell reached 35.24% efficiency, certified by SIMIT. This represents JinkoSolar’s 34th world record across cells and modules, arriving just five months after its previous milestone on the same architecture.

Stripping away press-release optimism, we examine the underlying device physics, the metrological boundaries of this announcement, and what it practically means for R&D, materials, and procurement teams.

01 Fact-Check Matrix: Verified Disclosures vs. Undisclosed Parameters ​

Before evaluating technical depth, we separate confirmed first-party facts from engineering parameters that remain unverified.

Evaluation DimensionDisclosed InformationVerification Status & Engineering Notes
Source & DateJinkoSolar official website, Nov 19, 2026 (CST)Verified (Tier-A corporate primary release)
Certified Efficiency35.24% (N-type TOPCon/perovskite tandem)Partially Verified (Official release checked; original certificate not reviewed)
Certifying BodySIMIT, Chinese Academy of SciencesVerified (Same certifying lab as the prior 34.82% record)
Prior Benchmark34.82% (Released June 16, 2026; 33rd record)Verified (156-day interval; +0.42 pct gain)
Cell Active AreaUndisclosed (Lab-scale ~1 cm² vs. commercial wafer size unspecified)To Be Verified (Area strongly impacts series resistance and uniformity)
I-V Scan ProtocolUndisclosed (Forward/reverse hysteresis and steady-state MPPT not stated)To Be Verified (Ion migration in perovskites can inflate transient I-V scans)
Encapsulation & Cert IDUndisclosed (Unencapsulated vs. encapsulated state and certificate number omitted)To Be Verified (Bare-cell peak efficiency differs from packaged reliability)
Commercialization ClaimDescribed as "key progress from lab efficiency toward industrialization"Corporate Opinion (Not a verified mass-production readiness metric)

Notably, because both the 34.82% and 35.24% figures were certified by SIMIT, the longitudinal comparison carries solid internal consistency—indicating genuine reductions in optical and recombination losses within JinkoSolar’s internal iteration baseline over the past five months.

Figure 1. Change in announced tandem cell efficiency

Figure 1. Change in announced tandem cell efficiency

02 Breaking Down the Four Disclosed Technologies: Why TOPCon Tandems Hinge on Textures and Interfaces ​

Unlike heterojunction (HJT) bottom cells—which natively feature a transparent conductive oxide (TCO) layer that interfaces smoothly with perovskite top cells—N-type TOPCon tandems face a tougher trade-off between leveraging the massive installed base of TOPCon manufacturing lines and managing surface morphology at the recombination junction.

JinkoSolar’s four highlighted technologies map directly onto the core loss channels of a TOPCon tandem:

1. Selective Passivation on Textured N-Type TOPCon Silicon ​

Industrial TOPCon wafers rely on micron-scale random pyramids for light trapping. Depositing a sub-micron perovskite layer directly onto large pyramids risks incomplete coverage and pyramid-tip shunting (collapsing shunt resistance, Rsh). Conversely, polishing the front surface flat spikes optical reflection and hurts bottom-cell current.

Selective passivation aims to preserve light-trapping geometry while tailoring dielectric/passivation coverage across pyramid peaks, valleys, and crystal facets. Done properly, this preserves high open-circuit voltage (Voc) in the TOPCon bottom cell while providing low-resistance carrier transport into the recombination layer.

2. Synchronized Multi-Component Perovskite Crystallization ​

To split the solar spectrum optimally with a 1.12 eV silicon bottom cell, the perovskite top cell requires a wide bandgap (~1.68 eV), typically achieved using mixed-cation and mixed-halide (Br/I) compositions.

On rough, micron-textured substrates, solution or hybrid vapor-solution deposition often suffers from asynchronous crystallization kinetics—leading to thickness non-uniformity between valleys and tips, pinholes, and halide phase segregation. Synchronized crystallization uses additive engineering and controlled nucleation kinetics so all components crystallize uniformly across uneven topography, minimizing grain-boundary defects and residual film stress.

3. Nanoscale Interfacial Passivation Materials ​

The buried and top interfaces between the perovskite absorber and charge-transport layers (ETL/HTL) dominate non-radiative recombination and serve as primary initiation sites for ion migration under illumination and electrical bias.

Introducing nanoscale passivation layers—such as self-assembled monolayers (SAMs) or functionalized dipolar molecules—chemically passivates undercoordinated Pb2+ and halide vacancies while tuning energy-level alignment without adding parasitic series resistance. This is a critical lever for pushing both Voc and fill factor (FF) beyond the 34% threshold.

4. Enhanced Optical Management ​

In a two-terminal (2T) monolithic tandem, the top and bottom subcells are connected in series, meaning total current is bottlenecked by the current-limiting junction. Optical management encompasses anti-reflection coating (ARC) refractive-index matching, minimizing parasitic free-carrier absorption in the recombination layer, and boosting near-infrared reflectance on the rear of the TOPCon cell to maximize current matching.

Figure 2. Disclosed technologies and corresponding loss mechanisms

Figure 2. Disclosed technologies and corresponding loss mechanisms

03 Metrological Boundaries: Why 35.24% Cannot Be Cross-Compared Directly ​

A common pitfall in PV news coverage is ranking headline efficiency numbers from different testing protocols on the same leaderboard.

Under IEC 60904-1-1:2017 (multi-junction I-V measurement) and IEC 60904-1:2020 (general I-V measurement principles), tandem metrology is substantially more complex than single-junction silicon testing. Without the full certificate, three strict boundaries apply:

  1. Area Scaling (1cm2 vs. Commercial M10/G12 Wafers): Record lab cells typically use small designated aperture areas (~1cm2) where sheet-resistance losses and coating non-uniformities are negligible. Scaling to full commercial wafer formats introduces dead-area losses, metallization shading, and film uniformity penalties that typically reduce efficiency by several percentage points.
  2. Transient I-V Sweep vs. Stabilized MPPT: Perovskites exhibit pronounced capacitive behavior and mobile-ion hysteresis. While IEC 60904-1-1:2017 mandates Class AAA multi-source simulators with spectral mismatch correction to ensure accurate subcell current matching, authoritative international tables (e.g., NREL or Nature-level certified benchmarks) increasingly require stabilized maximum power point tracking (MPPT) verification. Until steady-state certification is confirmed, this 35.24% figure should not be directly compared against certified stabilized records (such as 34.71% benchmarks).
  3. Lab Efficiency vs. Field Durability: Crossing 35% on an unencapsulated or lab-sealed cell is fundamentally distinct from passing IEC 61215-2:2021 damp heat (DH1000), thermal cycling (TC200), and multi-year outdoor exposure—where low-WVTR encapsulation (POE/butyl edge seals), low-temperature interconnection, and reverse-bias/PID resilience remain decisive hurdles.

04 Tiered Takeaways for PV Practitioners ​

  1. Cell R&D & Process Engineers: The battleground for TOPCon tandems has shifted from feasibility to line-compatible textured-wafer processing. Keep close watch on low-temperature process budgets (typically <150°C for top-cell layers to prevent thermal degradation) and large-area uniformity in vapor-assisted or hybrid deposition.
  2. Materials & Equipment Suppliers: Two of the four cited innovations point directly to nanoscale interfacial passivators and crystallization additives. High-purity charge-transport molecules, low-damage TCO sputtering targets, and wide-web deposition tools capable of conformal coating over micron-scale pyramids represent high-conviction supply-chain opportunities.
  3. Reliability, Certification & Procurement Teams: Adopt a "4-Point Tandem Audit Checklist" whenever evaluating 34%+ or 35%+ efficiency announcements: (1) What is the designated active area? (2) Is the figure an I-V scan average or stabilized MPPT output? (3) Was the device encapsulated, and what is its post-test retention? (4) Are the certificate ID and spectral mismatch factors traceable? Only records passing all four checks belong in a formal technology evaluation matrix.

05 Balanced Assessment: Strategic Signal vs. Unanswered Questions ​

Objectively, lifting N-type TOPCon/perovskite tandem efficiency from 34.82% to 35.24% in five months sends two constructive signals: first, TOPCon—the industry’s dominant installed manufacturing base—retains a high, actively expanding efficiency ceiling for tandem upgrades; second, sustained Tier-1 investment in interface and optical engineering is steadily narrowing the gap between lab concepts and pilot-line readiness.

At the same time, engineering discipline requires restraint. Without quantitative process windows, area disclosures, or aging curves, the distance between a 35.24% lab certification and a bankable 25-year commercial module is not measured in tenths of a percentage point—it is defined by full-area yield, low-temperature metallization economics, and long-term environmental stability.

One-Sentence Conclusion

JinkoSolar’s certified 35.24% efficiency reinforces the high-ceiling upgrade potential of N-type TOPCon/perovskite tandems, but until cell area, steady-state MPPT protocol, and encapsulation stability data are disclosed, it should be treated strictly as a milestone in laboratory efficiency rather than a direct proxy for commercial readiness or outdoor performance.

Methodology & Data Notes ​

  1. Absolute Efficiency Gain: $35.24\% - 34.82\% = +0.42\text{ percentage points (pct)}$.
  2. Relative Efficiency Gain: $(35.24 - 34.82) \div 34.82 \times 100\% \approx +1.21\%$.
  3. Time Interval & Pace: 156 calendar days between the June 16, 2026 (34.82%) and November 19, 2026 (35.24%) announcements (~5 months), averaging approximately +0.084pct/month over this window.
  4. Verification Scope: Efficiency figures, technical descriptions, and certifying institution details are sourced from JinkoSolar’s official press releases (Tier-A corporate primary source). Because the original SIMIT test certificate was not publicly accessible at the time of writing, undisclosed parameters (active area, scan mode, encapsulation status) are explicitly flagged as unverified with zero assumptions extrapolated.

References ​

  1. JinkoSolar Official News Release, JinkoSolar Perovskite/TOPCon Tandem Solar Cell Efficiency Reaches 35.24%, November 19, 2026, [https://www.jinkosolar.com/site/newsdetail/3470\](https://www.jinkosolar.com/site/newsdetail/3470)
  2. JinkoSolar Official News Release, 33rd World Record! JinkoSolar Sets New Perovskite/TOPCon Tandem Cell Efficiency Record of 34.82%, June 16, 2026, [https://www.jinkosolar.com/site/newsdetail/3218\](https://www.jinkosolar.com/site/newsdetail/3218)
  3. IEC 60904-1-1:2017, Photovoltaic devices – Part 1-1: Measurement of current-voltage characteristics of multi-junction photovoltaic (PV) devices
  4. IEC 60904-1:2020, Photovoltaic devices – Part 1: Measurement of photovoltaic current-voltage characteristics
  5. IEC 61215-2:2021, Terrestrial photovoltaic (PV) modules – Design qualification and type approval – Part 2: Test procedures

PV Materials Lab | 光伏新材料研究所 Website: [https://pvmaterialslab.com](https://pvmaterialslab.com)

Disclaimer:

  1. This article is independently authored by the PV Materials Lab team based on publicly available authoritative sources and first-principles engineering analysis for industry knowledge sharing.
  2. Corporate disclosures and claims are explicitly attributed with their verification status; this article constitutes neither a commercial endorsement nor a critique of any specific enterprise or technology route.
  3. Unverified testing parameters (such as active area, steady-state output, and long-term degradation data) are clearly bounded; readers should rely on complete third-party test reports for technical selection or procurement decisions.
  4. Republication and industry discussion are welcome with attribution to "PV Materials Lab (pvmaterialslab.com)".