Frame Manufacturing: From Aluminum Billet to Finished Frame
PV Module Frame Series · 05

A PV frame goes through a chain of steps between aluminum ingot and module: casting, extrusion, quenching, aging, surface treatment, precision cutting, punching and corner assembly. In the fifth article of our frame series, we walk through what each step controls and what tends to go wrong, focusing on porthole dies and weld seams, 45° miter cuts and corner-key crimping, and the key quality checkpoints: dimensional tolerance, hardness, film thickness, burrs and electrical continuity at the corners.
The first four articles covered the frame's function, material, surface treatment and structural design, all about what a frame should be. This one is about how it is made: what steps does a frame pass through from aluminum ingot to module, and what does each step control? Many problems that surface only at the module factory were planted upstream.
01 A frame's journey: the whole process
Industry reports usually summarize PV frame production in four stages: casting, extrusion, anodizing and further processing. Expanded, the main steps are as follows:

Figure 1 Main production steps of an aluminum PV frame
Two features of this flow are easy to overlook. First, the order cannot change: aging must come before surface treatment, and surface treatment before precision cutting and punching, which is why, as Article 03 noted, cut ends and hole walls have no film protection. Second, corner assembly usually happens at the module factory: the frame maker typically delivers long and short profiles that are already cut and punched, sometimes with corner keys pre-inserted, and the four sides are joined into a frame during the framing step.
02 Casting and extrusion: laying the foundation
Casting melts aluminum ingot with magnesium, silicon and other master alloys, adjusts the composition to the alloy grade, degasses, removes dross, filters, and casts cylindrical billets. Billets are then usually homogenized: held at high temperature for a period so magnesium and silicon distribute more evenly, removing segregation from casting. Good homogenization allows faster extrusion and steadier surface quality.
Problems planted at casting often show up only later: incomplete degassing leads to blisters after extrusion; inclusions cause surface defects that become more visible after anodizing; composition swings directly affect later strength and hardness. The impurity control for recycled aluminum discussed in Article 02 is enforced mainly at this step.
Extrusion places the heated billet in a container and uses thousands of tonnes of force to push it through a die, producing a continuous profile much like squeezing toothpaste. Because a frame section contains a closed cavity, it requires a porthole die: the aluminum flow is split into several streams around the mandrel that forms the cavity, then “welded” back together in the welding chamber.

Figure 2 Porthole-die extrusion and weld seams
This creates a hidden risk specific to hollow frames: weld seams. Where the metal streams rejoin, the microstructure differs slightly from the rest. If welding is poor, strength here is lower and the profile may crack along the seam under load; after anodizing, a visible color line may also appear. Die design, extrusion temperature and speed all affect weld quality.
As the profile leaves the die it is press-quenched immediately (as Article 02 explained, this step decides T5 versus T6), then pulled, stretch-straightened and finally sawn into stock lengths for aging.
03 Aging and surface treatment: setting strength and “clothes”
The stock lengths are loaded into an aging oven and held at temperature for several hours to precipitate strengthening phases, bringing strength and hardness to spec. Whether the oven temperature is uniform and the baskets are loaded sensibly decides whether hardness is consistent across one batch.
After aging comes surface treatment: pretreatment such as degreasing, alkaline etching or chemical polishing, then anodizing and sealing, or e-coating or powder coating. Article 03 covered film thickness and sealing, so we add just one point here: pretreatment sets the base tone of the appearance. Over-etching makes the surface look whitish and reduces dimensions, while under-treatment can leave spots and color variation.
04 Precision cutting and punching: millimeter-level accuracy
Surface-treated stock lengths then go into further processing. First comes precision cutting: the stock is cut into long and short sides to suit the module size, with ends usually mitered at 45° so that the four sides butt together at neat corners.
The gap between frame and laminate is only a few millimeters. A small error in side length or miter angle leads to corner gaps, out-of-tolerance diagonals, or even a frame that will not fit. So precision cutting places strict demands on saw-blade condition, positioning accuracy and cutting speed.
Next comes punching: presses and dies punch mounting, grounding and drain holes in Face C, and sometimes holes or notches for fixing the corner keys. The most common problem here is burrs:
- Scratch risk: burrs can injure operators and scratch the film on other profiles during handling and framing;
- Installation issues: burrs at hole edges keep bolts and grounding washers from seating properly, which affects grounding reliability;
- Deformation: with die wear or improper clearance, hole edges can dent or flare, especially on thin-walled profiles.
05 Corner keys and corner assembly: the frame's four joints
Corner keys join the four profiles into a frame. A corner key is inserted into the cavities of two adjacent sides and locked by crimping: a punch dents the outer wall of the profile so that it deforms locally and bites into the key.

Figure 3 45° miter cut, corner-key insertion and crimping
The common corner-key options are roughly as follows:
| Option | Method | What to watch |
|---|---|---|
| Aluminum key + crimping | Slices of extruded key profile, crimped after insertion | Most common; number, position and depth of crimp points |
| Toothed or barbed press-fit key | Held by interference fit and tooth engagement | Balance between insertion and pull-out force |
| Keys of other materials | Steel or engineering-plastic keys, mostly in special frame designs | Strength, corrosion and conductivity need separate verification |
Corner quality comes down to several things: corner strength, i.e. how much pulling and twisting the corner can take; squareness, i.e. whether the diagonal difference is within tolerance; corner gaps, where large gaps trap water and salt and, as Article 03 explained, become hot spots for crevice corrosion; and the easily overlooked electrical continuity across the corners.
The equipotential bonding continuity test in IEC 61730-2 checks continuity from the designated grounding point to the farthest exposed conductive part. If only one side has a grounding hole, conduction to the other three sides relies on the corner joints. The metal-to-metal contact formed when crimping pierces the anodic film is part of that conductive path. Also, as Article 02 noted, profiles that are too hard crack more easily at the crimp points.
Takeaway: A corner key is small, yet it ties together strength, dimensions, corrosion and grounding. Judge corner quality not by whether it went together, but by whether it pulls apart, leaks or fails to conduct.
06 Key quality checkpoints: control at the source
Here are the key quality checkpoints across the whole process:
| Checkpoint | Main checks | Source of problems |
|---|---|---|
| Chemical composition | Mg, Si, Fe, Cu content | Casting |
| Dimensional tolerance | Section dimensions, length, miter, diagonals | Extrusion, cutting |
| Hardness and strength | Webster hardness, tensile properties, batch consistency | Quenching, aging |
| Film thickness and sealing | Average and local thickness, sealing quality | Surface treatment |
| Appearance | Scratches, color variation, weld seams, blisters | Casting, extrusion, surface treatment |
| Holes and burrs | Hole dimensions, burr height, hole-edge deformation | Punching |
| Corner quality | Corner strength, gaps, continuity | Corner keys, crimping, framing |
The last column deserves a second look: most frame problems seen at the module factory originate in some step at the frame maker. Incoming inspection catches some of them, but a more effective approach is to work with suppliers to build key parameters into process control, such as aging-oven temperature records, die-life management and regular checks of punching dies.
Bottom line: Frame quality is built in, not inspected in. Rather than picking out problems at incoming inspection, work with suppliers to control the key process steps.
07 Final thoughts
To wrap up this article:
- Casting: sets composition and internal quality; blisters, inclusions and impurities all start here;
- Extrusion: porthole dies make hollow sections possible but bring the weld seam, a risk specific to hollow frames;
- Aging and surface treatment: fix the strength and the “clothes”, and the order cannot change;
- Cutting and punching: millimeter-level accuracy decides whether framing goes smoothly, and burrs affect safety and grounding;
- Corner keys and assembly: tie together strength, dimensions, corrosion and grounding.
Once the frame is made, the last step is to assemble it with the laminate. In the next article we cover module framing: how to choose between silicone and double-sided tape, how a framing machine works, and how to avoid common defects such as squeeze-out, missing adhesive and corner gaps. Stay tuned.
Calculation notes / data basis
- Public industry reports only summarize PV frame production as four stages (casting, extrusion, anodizing, further processing) and give no step parameters. The expanded steps, common problems and checkpoints in this article are our summary of common industry practice; process routes and parameters vary between companies.
- “Corner assembly mostly happens at the module factory, and frame makers often pre-insert corner keys” summarizes a common delivery practice; the actual arrangement depends on the agreement between the parties.
References
- 观研报告网. 我国光伏边框行业现状及趋势分析, 2023-05. https://www.chinabaogao.com/market/202305/634481.html
- T/SHLX 005—2024 太阳能电池边框用铝合金型材 / Aluminum alloy extruded profiles for solar cell frames
- GB/T 5237.1 铝合金建筑型材 第1部分:基材 / Aluminium alloy extruded profiles for architecture – Part 1: Substrate profiles
- IEC 61730-2 Photovoltaic (PV) module safety qualification – Part 2: Requirements for testing (MST 13 equipotential bonding continuity test)
PV Materials Lab
https://pvmaterialslab.com
PV Materials Lab
A PV R&D and technical team with 10+ years of experience | In-depth technical knowledge sharing
Materials · Reliability · Failure Analysis · Standards & Certification · Products · Processes
Exploring AI + PV — collaboration welcome
Disclaimer:
- Original content reflects the authors' personal views only, is for reference, and does not constitute investment advice.
- Reposted and cited content is credited to its source, with respect for original work.
- Some content is AI-assisted (chart generation, data retrieval, concept explanations, etc.); the core framework and key content are written by our technical team and reviewed by humans.
- For any inaccuracy or infringement, please leave a message or contact us.