Frames and Module Reliability: Common Failure Modes
PV Module Frame Series · 08

When a frame goes wrong, it rarely stays the frame's problem alone; glass, cells and grounding safety are often dragged in. In the eighth article of our frame series, we sort frame-related failures into mechanical, corrosion and electrical types: lower-frame deformation and glass breakage from non-uniform snow, corner cracking and loosened corner keys, coating degradation and galvanic corrosion, and grounding failure and PID, ending with a troubleshooting table from symptom to root cause.
The first seven articles covered the frame's whole journey from design and manufacturing to testing. But passing in the lab does not mean nothing goes wrong outdoors. This article takes another angle and starts from failure: what do frame-related problems look like in the field, what mechanisms are behind them, and where should we look for root causes?
01 Start with a failure map
Frame-related failures fall roughly into three groups by mechanism:
- Mechanical: frame deformation, corner cracking, loosened corner keys, glass slipping out of the slot and broken glass corners;
- Corrosion: coating degradation, corrosion at cut ends and holes, crevice corrosion and galvanic corrosion;
- Electrical: loss of grounding continuity, and PID (potential-induced degradation) linked to frame grounding.

Figure 1 Where common frame-related failures occur
These three groups often feed each other: a cracked corner traps water and speeds up corrosion; corrosion raises contact resistance and leads to grounding failure. So in failure analysis, do not fixate on the most visible symptom.
02 Lower-frame deformation and glass breakage: the non-uniform snow test
In snowy regions there is a typical failure: the frame along the module's lower edge bends and rolls outward, and the glass starts breaking from the lower corners. The reason is that snow is not distributed evenly.
On a tilted module, snow slides downward. For modules whose lower frame stands above the glass surface, that frame acts like a “snow dam”, holding snow at the lower edge where it piles up ever deeper. As a result, the load concentrates near the lower frame and has a component acting down the slope, pushing the lower frame outward and downward. This is completely different from wind or snow pressure spread evenly over the whole module.

Figure 2 Forces from non-uniform snow piling at the module's lower edge
To address this failure, the IEC published IEC 62938, non-uniform snow load testing for PV modules, in 2020. According to the standard's abstract, it applies to framed modules whose lower frame protrudes beyond the front glass after installation and blocks snow from sliding off; a prerequisite is that the module has already passed the IEC 61215-2 static mechanical load test with a front load of at least 5400 Pa. In other words, withstanding a uniform 5400 Pa does not mean withstanding non-uniform snow.
Design countermeasures include strengthening the lower frame section, especially its stiffness against rolling outward; reducing how far Face A stands above the glass, or adopting features that help snow slide off; adding back support bars in heavy-snow regions; and specifying tilt ranges and snow-clearing precautions in the installation manual.
Takeaway: Uniform load tests measure how much force a module takes; non-uniform snow tests measure where that force concentrates. In snowy regions, the lower frame is the real weak link.
03 Corner cracking and loosened corner keys
The corners are where the four profiles connect, and where stress concentrates. Two corner failures are common: cracked corner profiles, and loosened corner keys with opened corners.
Tracing root causes often leads back to steps covered in earlier articles:
- Material: profiles that are too hard and lack ductility develop microcracks at crimping, which grow under repeated thermal cycling and wind load (Article 02);
- Manufacturing: poor fit between corner key and profile cavity, or too few or too shallow crimp points, leaves too little locking force (Article 05);
- Framing: improper pressing force or corner parameters leave gaps or initial stress at the corners (Article 06);
- Load: repeated flexing from long-term wind vibration amplifies any of these initial defects.
An opened corner is not just cosmetic: the gap traps water and salt, causing crevice corrosion; loosened corners lower the frame's overall stiffness; and if other sides rely on the corners for grounding continuity, grounding reliability may suffer as well.
04 Corrosion: coating degradation and galvanic corrosion
Frame corrosion comes in two kinds. The first is degradation of the coating itself: poorly sealed anodic films develop white spots and chalking in damp heat and salt mist, while cut ends, hole walls and scratches are bare aluminum and often show white corrosion products first. Article 03 covered this in detail.
The second is the more hidden galvanic corrosion. When two metals with different electrode potentials touch directly, and rain, condensation or salt mist forms an electrolyte, they make a tiny battery: the more active metal with the lower potential becomes the anode and corrodes, while the nobler metal is protected.

Figure 3 Galvanic corrosion between an aluminum frame and a stainless-steel fastener
Aluminum is more active than both stainless steel and copper, so in these pairings it is usually the aluminum frame that corrodes. Common contacts in the field include frames with stainless-steel bolts and clamps, frames with copper grounding wires, and frames with steel racking. In coastal, humid, agrivoltaic and livestock settings the problem is markedly worse.
There are three main remedies: insert insulating washers or isolation layers between dissimilar metals; choose material pairings with smaller potential differences; and connect copper grounding wires through tin-plated lugs or dedicated copper-aluminum transition fittings rather than clamping them directly onto the aluminum frame.
05 Electrical failures: grounding and PID
Grounding failure is the frame failure with the most serious consequences yet the least visibility. It causes no obvious energy loss, but once insulation inside the module fails, unreliable grounding can leave the frame live, posing a safety risk to people. Common causes include grounding washers that never pierced the anodic film, contact points whose resistance rises through long-term corrosion, and loosened corners that cut the other three sides off from conduction.
We discussed the link between frames and PID in our PID series. In short, the system's high voltage creates a potential difference between the grounded frame and the cells, which is one of the necessary conditions for PID; the leakage current in turn depends on glass surface moisture, soiling and the distance between cells and frame. In real plants, PID often appears first in cells near the frame, especially along the lower edge where water and dirt collect.
06 From symptom to root cause: a troubleshooting table
Here is the above condensed into a troubleshooting table for quick diagnosis during plant inspections or complaint analysis:
| Symptom | Check first | Possible root cause |
|---|---|---|
| Lower frame rolled out, glass broken at lower corner | Snow conditions, tilt angle | Non-uniform snow, weak lower frame |
| Permanently bent frame | Mounting per manual? | Shifted mounting points, low section margin |
| Cracked corners | Profile hardness, crimp points | Excess hardness, wrong crimp parameters |
| Opened corners, loose keys | Corner quality, diagonals | Poor key fit, wrong framing parameters |
| White spots, chalking | Film thickness, sealing | Poor sealing, thin film |
| Severe local corrosion at contacts | Materials in contact | Galvanic corrosion, no isolation |
| High grounding resistance | Grounding point, corner continuity | Unpierced film, corroded contacts |
| Power loss in cells near frame | EL images, system voltage and grounding | PID |
Bottom line: Frame failures rarely have a single cause. From the symptom, trace back along the chain of material, manufacturing, framing, installation and environment to find the real root cause.
07 Final thoughts
To wrap up this article:
- Three failure types: mechanical, corrosion and electrical failures often feed each other, so look at the whole picture;
- Non-uniform snow: snow piling at the lower edge concentrates load on the lower frame; passing a uniform 5400 Pa does not guarantee survival, and IEC 62938 targets exactly this;
- Corner failures: root causes often lie in profile hardness, crimping and framing parameters;
- Galvanic corrosion: aluminum is more active than stainless steel and copper, so dissimilar metals in contact must be isolated;
- Grounding and PID: grounding failure is the most serious yet least visible, and PID often starts in cells near the frame.
Knowing how frames fail, we can now discuss the limits of cost reduction. In the next article we look at frame weight reduction and “moving beyond aluminum”: how much lighter aluminum frames can get, and what advantages and hidden risks steel and composite frames bring. Stay tuned.
Calculation notes / data basis
- The scope and prerequisite of IEC 62938 (passing MQT 16 with a front load of at least 5400 Pa) are taken from the iTeh catalog abstract of EN IEC 62938:2020; the full standard was not obtained, so follow the standard text for test methods and criteria.
- That aluminum is more active than stainless steel and copper is a general conclusion from the galvanic series; actual corrosion rates also depend on area ratio, electrolyte and environment.
- “PID often appears first in cells near the frame” is a common industry observation; the actual distribution depends on module construction, system voltage and environment.
References
- IEC 62938:2020 Photovoltaic (PV) modules – Non-uniform snow load testing(iTeh 标准目录摘要). https://standards.iteh.ai/catalog/standards/clc/f8477d09-3248-4d95-873e-92734a898c33/en-iec-62938-2020
- IEC 61215-2:2021 Terrestrial photovoltaic (PV) modules – Design qualification and type approval – Part 2: Test procedures (MQT 16)
- IEC 61730-2 Photovoltaic (PV) module safety qualification – Part 2: Requirements for testing
- IEC 61701 Photovoltaic (PV) modules – Salt mist corrosion testing
- Greentech Renewables. Galvanic corrosion and protection in solar PV installations. https://www.greentechrenewables.com/article/galvanic-corrosion-and-protection-solar-pv-installations
PV Materials Lab
https://pvmaterialslab.com
PV Materials Lab
A PV R&D and technical team with 10+ years of experience | In-depth technical knowledge sharing
Materials · Reliability · Failure Analysis · Standards & Certification · Products · Processes
Exploring AI + PV — collaboration welcome
Disclaimer:
- Original content reflects the authors' personal views only, is for reference, and does not constitute investment advice.
- Reposted and cited content is credited to its source, with respect for original work.
- Some content is AI-assisted (chart generation, data retrieval, concept explanations, etc.); the core framework and key content are written by our technical team and reviewed by humans.
- For any inaccuracy or infringement, please leave a message or contact us.